Main component:Zirconium
Gross density:6g/cm^3
Flexural Strength:1000 Mpa (Psi*103)
Material:Zirconium
Gross density:6g/cm^3
Fracture Toughness:7 Mpa m1/2
Main component:zirconium
Vickers Hardness:1300 HV0.5
Maximum Operating Temperature:1200 ℃
Material:Yttria-stabilized zirconia
Density:6g/cm^3
Thermal Conductivity:4 W/mK
Coefficient of Linear Expansion (20–400°C):10 10^–6/℃
Young’s Modulus (dynamic)/Elasticity Modules:205 Gpa
Gross density:6g/cm^3
Density:6g/cm^3
Material:Zirconium
Volume Resistivity:>10^15 100°
Gross density:3.7g/cm^3
Color:Brown
Main component:95% Al2O3 or 95& alumina
Main Ingredient:95% alumina
Bending Strength:210 Mpa
Density:≥3.7g/cm3
Material:95% alumina ceramic
Maximum Operating Temperature:1000 ℃
Thermal Shock Resistance:250℃ Tc
Alkali Resistance:mg/cm^2 ≤0.2
Acid Resistance:mg/cm^2 ≤0.7
Main component:95% Al2O3
Material:95% Alumina
Gross density:3.7g/cm^3
Young’s Modulus (dynamic)/Elasticity Modules:300 Gpa
Material grade (%Al2O3 content):96%
Bulky density (fired), Mg/m3):3.8
Rockwell hardness(R45N):86